The thermal conductivity of titanium alloys typically ranges from about 6 to 20 W/m·K, depending on the specific alloy composition and heat treatment. The table below provides a comprehensive list of thermal conductivity values for various titanium alloys at room temperature (approximately 20°C or 68°F).

Click on the icon to switch between SI (W/m·K) and Imperial (BTU/h·ft·°F) units.

Thermal Conductivity of Titanium Alloys
UNS numberComposition
Grade 1R5025016
Grade 2R5040016.4
Grade 3R5055019.9
Grade 4R5070017.2
Grade 5R56400Ti-6Al-4V6.7
Grade 6R54520Ti-5Al-2.5Sn7.8
Grade 7R52400Ti-0.2Pd16.4
Grade 9R56320Ti-3Al-2.5V8.3
Grade 10R58030Ti-11.5Mo-6Zr-4.5Sn6.28
Grade 11R52250Ti-0.2Pd17
Grade 12R53400Ti-0.3Mo-0.8Ni19
Grade 18R56322Ti-3Al-2.5V-0.06Pd7.6
Grade 19R58153Ti-8V-6Cr-4Mo-4Zr-3Al6.2
Grade 21R58210Ti-15Mo-3Al-2.7Nb-0.25Si7.6
Grade 23R56401Ti-6Al-4V (ELI)6.7
Grade 32R55111Ti-5Al-1Sn-1Zr-1V-0.8Mo7.5
Grade 35R563407.4
Grade 36R58450Ti-45Nb10
Grade 38R542508
Timetal® 21SR58210Ti-15Mo-3Nb-3Al-0.2Si7.6
Timetal® 6-2-4-2R54620Ti-6Al-2Sn-4Z r-2Mo6
Timetal® 6-6-2R56620Ti-6Al-6V-2Sn7.2
Timetal® 230Ti-2.5Cu12.97
References: 1) Cardarelli, François. Materials Handbook: A Concise Desktop Reference. Switzerland: Springer International Publishing, 2018.